Using the Stoll Abrasion test, we compared our 1050 ballistic nylon to the 1680 ballistic used by our
competitors. The 1680 denier fabric failed after only 1055 cycles (black fabric); our 1050 denier fabric (red fabric) didn't fail until 2110 cycles.
|
Their 1680 fabric after only 1055 cycles.
|
Our 1050 fabric after 2110 cycles.
|
Bottom line: our ballistic fabric is twice as abrasion resistant as the competitors.
| |